Mark, You wrote: >I would also advise you to make sure the Hydrocote is stirred >very well. >... >... open the lid, stir it, get what you need out, >and then reseal the lid. I am down to near the bottom of the quart can of Hydrocote I first purchased, and I think I've noticed a viscosity increase. I now usually stir the PUR just before using, but admit that I have not always been so vigilant. It may also be that the air in the can, with repeated openings, causes some viscosity increase. At an rate, the symptoms I see are streaks in the coating that were not there before. It is the same type of streaking I saw with Liquitex acrylic before I diluted it 3:1. Paul http://www.PaulRoark.com