On Fri, 02 Sep 2005 02:07:31 +0200, johnwhitneyfiat <johnwhitneyfiat@...> wrote: > I have been off the group for a while and I'm sure this was covered. > In the direction for making etchant from Hydrogen Peroxide and Muratic > Acid, it says that you can regenerate with a bubbler. How long does > this take? I know it will depend on the amount and the area that was > etched, but is there a rule of thumb to make it work. I do have to day > that I make a small bathch and it worked great on a sample board. > John Whitney > Wis X 1/9 I personally never tried it, but i would say many hours, perhaps days. My tank volume isn't that large, and that means if i run out of active etchant halfway through a board i have to do something, waiting very long until it is regenerated is not an option. So i just add a small amount of CuCl. With the low price of that stuff and tiny amounts required..... ST
Message
Re: [Homebrew_PCBs] Regenerating CuCl
2005-09-02 by Stefan Trethan
Attachments
- No local attachments were found for this message.