2005-12-02 by Mike Young

Datak says about Tinnit:

"4. After plating, the cirucit board will have chemical residues that will 
in time dull or corrode the plating. To neutralize and remove these 
residues, immerse and scrub the object in a mild solution of household 
ammonia, followed by running water rinse. Dry and polish with a paper 
towel."

FWIW.


----- Original Message ----- 
From: "derekhawkins" <derekhawkins@...>
>
> For what it's worth....I have a half bottle of Coolamp here, it was
> my "tinning" method of choice for a while. 4 to 5 year old tracks
> tinned with it now have a yellowish tint....Wouldn't waste my time on
> that again.