> In my Kepro datasheet, it says I can shock the solution by adding some spent > Sodium Persulfate so I don't have to wait for it to stabilize. > > I had some used solution which was 3 months old that I used to shock the > bath. I know the shelf life for etching is 3 weeks, but can it still be used > to add in adjusting the pH? > > I went ahead and etched, but it took forever. I was successful at 12/12, but > the etching seem to take 15 - 20 minutes. When I had my techs making proto > boards, it seemed we could etch in 3-5 minutes with hand agitation. The > solution was at 105-110 deg F. The board was quite small, and as I use huge > ground planes and leave > dead copper on the board to reduce waste, It seems it should have etched > close to the 3 minute time frame rather than 20 minutes. > > I'm doing tray etching with manual agitation. > > Thanks > Ron > >