On Mon, 06 Mar 2006 13:18:32 +0100, idaho_huckleberry <dmiller45@...> wrote: > What strength of HCL and H2O2 did you use? I went shopping for Muratic > > acid and found some at 37%, the H2O2 was 12% (listes as "40" on the > > side of the bottle) from my local Salon supply store. Are these stong > > enough to etch PCB's or should I look for stronger stuff? > > > Dave Miller the H2O2 is a bit weak, so will add more water, but it should work fine. You can freeze-concentrate H2O2, but i don't think it's needed. ST
Message
Re: [Homebrew_PCBs] Re: HCL + Peroxide Question
2006-03-06 by Stefan Trethan