Last night I added 1 litre of HCl (30.5%) to 2 litres of distilled water to make 12 litres of 10% etchant (to start off with) in my plastic Coleman cooler tank. To this I added 1.8 kg of clean copper wire I had washed in dish detergent and hot water. Twelve hours later, the copper covered with the acid solution looks unchanged. About half the wire, which is pieces about 12" long bent into different shapes, (so the copper is a large jumble), sticks out of the solution. Most of this is covered by a pink coloured, hazy looking film. I don't know what to expect, but so far this is what I have noted. Grant
Message
Starting CuCl etchant from scratch
2003-04-13 by grantfair2001