Stefan Trethan wrote: > The etchant will only keep as long as it is regenerated (usually with > oxygen from H2O2 or air). > > Especially with 3% H2O2 it is said to be hard/impossible to regenerate > this etchant as it adds too much water in the long run. I thought we also said the bubbler found in many etching tanks does this function to regenerate the etchant - and anyway in France it seems it's easy to find 35% H2O2... Anyway - I like this etchant. I would never use FeCl anymore :) bye as
Message
Re: [Homebrew_PCBs] Re: What is the best etching solution;
2009-04-26 by Alessio Sangalli