On 22/03/2010 18:35, Mark Lerman wrote: > As I understand it, the H2O2 is used to provide oxygen to the HCl, > but using 3% peroxide slows it down because of dilution of the > HCl. Has anyone tried just bubbling some oxygen through the HCl? Or > is this just too dangerous to contemplate?? Thought I'd ask before > trying.<smile> It's not all that dangerous, but you won't get much, if any, oxidisation. H2O2 is needed. Leon -- Leon Heller G1HSM
Message
Re: [Homebrew_PCBs] HCl Etchant Question
2010-03-22 by Leon Heller