On Mon, 22 Mar 2010 14:35:42 -0400, you wrote: >As I understand it, the H2O2 is used to provide oxygen to the HCl, >but using 3% peroxide slows it down because of dilution of the >HCl. Has anyone tried just bubbling some oxygen through the HCl? Or >is this just too dangerous to contemplate?? Thought I'd ask before >trying. <smile> Just bubble air. IIRC, it will convert to CUCL soon enough. That will require air to work. Harvey > >Mark > >
Message
Re: [Homebrew_PCBs] HCl Etchant Question
2010-03-22 by Harvey White