--- In Homebrew_PCBs@yahoogroups.com, Harvey White <madyn@...> wrote: > > On Mon, 22 Mar 2010 14:35:42 -0400, you wrote: > > >As I understand it, the H2O2 is used to provide oxygen to the HCl, > >but using 3% peroxide slows it down because of dilution of the > >HCl. Has anyone tried just bubbling some oxygen through the HCl? Or > >is this just too dangerous to contemplate?? Thought I'd ask before > >trying. <smile> > > Just bubble air. IIRC, it will convert to CUCL soon enough. That > will require air to work. > > Harvey > > > > >Mark > > > > > You have to get enough copper in it first, then air will work.