Na 1.10.2010 17:34, Philip Pemberton je pisal: > On 27/09/10 20:15, Hector Garcia wrote: >> Regenerate it >> >> http://www.qsl.net/iz7ath/web/02_brew/14_howto/02_clor/index.htm > Hmm, HCl+H2O2... isn't that the 'starter' for a CuCl etch bath? That is, > you mix HCl and H2O2, start up the air bubbler, then chuck in a few > chunks of copper and wait. > > So after that, you'd pretty much end up with a 'hybrid' etch bath, > consisting of FeCl3 and CuCl... interesting... Might explain why my etch > bath is going somewhat green. You need mode HCL and H2O2 to regenerate that. Just use straight HCL and H2O2 to etch board. > Would 9% H2O2 and 'brick cleaner' HCl be OK for this, or do I need > something more concentrated? For etching just use 9% H2O2 and HCL. One part HCL and aprox 3 part 9%H2O2. No water needed. Use as smal as you can quantity just to cover board. > Thanks,
Message
Re: [Homebrew_PCBs] Precipitate in ferric chloride storage bottle
2010-10-01 by Slavko Kocjancic
Attachments