I've posted this mixture before: Mix 3.8 grams of Stannous chloride into 1 liter of distilled water that is at 80 to 120 degrees fahrenheit in temperature. Stir well until dissolved. Add 49.5 grams of thiourea to the dissolved stannous chloride and distilled water while maintaing the temperature between 80 and 120 degrees fahrenheit. Stir well until dissolved. Add 12 ml of sulfuric acid to this mixture (Be careful! As you add the acid the mixture is going to get HOT! Also, Always, ALWAYS add acids to water. Never, NEVER add water to acids!). Stir well. You are now the proud owner of electroless tinning solution. Best regards Marvin Dickens Alpharetta, Georgia USA --- JanRwl@... wrote: Some > chemist "in here" please tell > us! > Jan Rowland ===== Registered Linux User No. 80253 If you use linux, get counted at: http://www.linuxcounter.org __________________________________ Do you Yahoo!? Free Pop-Up Blocker - Get it now http://companion.yahoo.com/
Message
Re: [Homebrew_PCBs] Re: how can i prevent corosion?
2003-12-01 by mpdickens
Attachments
- No local attachments were found for this message.