On Fri, 17 Dec 2004 23:19:59 +0000, Les Newell <lesnewell@...> wrote: > Hi, > I have been using CuCl etchant for a while now. Before etching I add a > tablespoon of 100 volume H2O2 and away I go. Recently something has > changed. When adding the H2O2 the soulution used to bubble slightly and > change colour from muddy green to a nice blue-green. Recently when I add > the H2O2 it bubbles violently and nothing else happens. Has anyone else > had this problem? > Perhaps I should just dump the solution and start again. > Les You have forgotten to add HCl. You did check the molarity from time to time, right? ;-) ST
Message
Re: [Homebrew_PCBs] CuCl wierdness
2004-12-17 by Stefan Trethan