--- In Homebrew_PCBs@yahoogroups.com, "Stefan Trethan" <stefan_trethan@g...> wrote: > > On Tue, 03 Jan 2006 16:37:32 +0100, Bruno St-Laurent <bsl88k@n...> > wrote: > > > > > > > I do use a bubbler !!!, ok, then i need to get concentrated H2O2!! is > > > > it easily available ??? > > > Yes, and not very expensive either. You want some around 30%. > I was afraid the london bombings might cause more restrictions on H2O2, > but so far i have not heard of any such thing. > > ST > Stefan how much H2O2 do i add ???? Bruno