Re: [Homebrew_PCBs] Re: CUCL Temperature , etch time ?????

2006-01-03 by Stefan Trethan

On Tue, 03 Jan 2006 17:40:03 +0100, Bruno St-Laurent <bsl88k@...>  
wrote:

>
>
> Stefan how much H2O2 do i add ????
>
>
> Bruno


Of the 30% stuff just a little bit. A spoon full or two (DO NOT USE  
METAL), 5ml or less i'd say. Basically the smallest amount i can pour with  
my H2O2 bottle. This regenerate enough etchant for one, maybe two or three  
boards, depending on size of course.