On Wed, 07 Feb 2007 17:45:41 +0100, scc_11067 <mr_cross@...> wrote: > Hi, I have found that inks don't hold up too against the muratic > acid/peroxide bath, > (even sodium and ammonia persulfates) > so i switched to ferric chloride > and get really good results. > I am currently using durabrite yellow with really good etch's > Could use durabrite magenta, but the ink bunches up on the board > if not dried instantly. > The persulfates just lift the ink off the board. > ( i printed and etched a sspcb that is smaller than a dime, just for > testing) > Fecl works best for direct ink printing IMHO. Interesting, i compared CuCl and FeCl, using a sample PCB just cut in half before etching, with MISPRO yellow, and could notice no significant difference between the two. My CuCl was very low molarity HCl though. ST
Message
Re: [Homebrew_PCBs] Re: C88 direct inkjet printing
2007-02-07 by Stefan Trethan
Attachments