> Adam wrote: > <SNIP> > I use alkaline ammonia chloride etchant because > I etch with electroplated tin as the etch > resists, and all acid etchants attack tin. > This etchant is very rare among hobbyists > because it really needs spray etcher or sealed > chamber to operate due to ammonia fumes. It > also needs complicated chemical analysis to > make sure it stays working. > Adam, have you dropped the CuCl in favour of the alkaline etchant because of problems with through hole plating ? Is the whole tent and etch thing problematic?
Message
Electroplated tin and PTH
2007-07-05 by Andrew