2008-01-31 by Markus Zingg

You definately positively don't need an over for dry-film laminating. 
You definately don't need it for the artwork develop etch cycle. You 
COULD use one in case the laminate is solder stop maks laminate but even 
there you can harden it using the UV exposure unit you need anways to 
work with laminate.

Markus