--- In Homebrew_PCBs@yahoogroups.com, Markus Zingg <homebrew-pcb@...> wrote: > > You definately positively don't need an over for dry-film laminating. > You definately don't need it for the artwork develop etch cycle. You > COULD use one in case the laminate is solder stop maks laminate but even > there you can harden it using the UV exposure unit you need anways to > work with laminate. > > Markus > > [snip] > > > > torture.. and for dry-film laminating you need an oven too, > > > yes, i was talking about soldermask dry-film. i've seen the dupont soldermask requieres uv+bake cure but bungard soldermask can be cured only with uv or both