Re: [Homebrew_PCBs] Tin - Plating

2008-06-04 by DJ Delorie

JanRwl@... writes:
> Doesn't that solution have to be warm (say 140°- 280° F or more) to work  
> well?

I've never heated it, seems to work OK.  No mention of heating on the
bottle either.