Stefan Trethan wrote: > Now there's your problem. You don't have CuCl, you have HCl and H2O2. > The one will keep, the other won't. > > You can make CuCl from HCL and H2O2 simply by etching copper, but > until you get there you have to add H2O2 each time you want to etch. > > Ah Ha, the rejuvination process, adding H2O2 before each etching session, until it becomes CuCl. Is that the stage where the solution changes color? Thanks guys for refreshing my ageing memory. Wayne
Message
Re: [Homebrew_PCBs] Shelf life of HCl/H2O2
2009-01-05 by Wayne Topa