Re: [Homebrew_PCBs] Re: Free bottle of Liquid Tin

2009-04-24 by Volkan Sahin

I think so, if it is steel it should work. I tried with x-acto knife blade and it worked. You need to touch with steel to copper traces a few seconds then it will start to generate bubbles (H2).   It is a little bit expensive electroless plating solution but easy to use. 
Cheers,
Volkan 


--- On Thu, 4/23/09, Mike Oyama <mikesb0x0fm4il2@...> wrote:

From: Mike Oyama <mikesb0x0fm4il2@...>
Subject: Re: [Homebrew_PCBs] Re: Free bottle of Liquid Tin
To: Homebrew_PCBs@yahoogroups.com
Date: Thursday, April 23, 2009, 7:49 PM











    
            
            


      
      Wow, Far out! I think I'll pick up one of those Electroless Nickel plating

kits then.



Could you use a wad of loose steel wool to activate the plating?



[Non-text portions of this message have been removed]




 

      

    
    
	
	 
	
	








	


	
	


      

[Non-text portions of this message have been removed]

Attachments

Move to quarantaine

This moves the raw source file on disk only. The archive index is not changed automatically, so you still need to run a manual refresh afterward.