2010-08-19 by Bob Macklin

I just bought the DATAK TinIt solution from All Electronics. They are dry 
crystals that you have to mix.

Bob Macklin
K5MYJ
Seattle, Wa.
"Real Radios Glow In The Dark"


----- Original Message ----- 
From: "fredbutz" <fredbutz@...>
To: <Homebrew_PCBs@yahoogroups.com>
Sent: Thursday, August 19, 2010 10:37 AM
Subject: [Homebrew_PCBs] Re: Now, tinning


I'm about to try the Sulfamic acid one.  I also got the chemicals on EBay. 
I'll let you know.


--- In Homebrew_PCBs@yahoogroups.com, Larry Battraw <lbattraw@...> wrote:
>
> > > > I have very good luck with elctroless tin. The formula I use came 
> > > > from the September 1971 issue of Ham Radio magazine.
> > > >
> > > > .5g Stannous Chloride
> > > > 2.0g Thiourea
> > > > 3.0g Sulfamic Acid
> > > > 100.0 mL Distilled water
> > > >
> > > > The solution is ued cold, I never tired heating it. It plates up in 
> > > > a few minutes and does a goog job but can't be use as a resist for 
> > > > further etching. The solution does not keep and I always make up a 
> > > > fresh batch for each board making session. I would usually mix up 
> > > > less than 100 mL depending on the size and number of boards I was 
> > > > doing.
> > > >
> > > > Craig
>
> Has anyone else tried this? I ordered the chemicals off eBay and
> tried it with sulfamic and sulfuric acid (separate times) and it does
> not seem to work. I was very careful measuring, used distilled water,
> and cleaned the copper with sandpaper so it was completely exposed.
> The recipe using sulfuric came from here:
> http://www.finishing.com/0200-0399/260.shtml
>
>  The only thing I can think of is that the Stannous Chloride I have is
> not actually what it seems to be since it's the only thing I haven't
> been able to substitute something else for. I tried a recipe for
> electroplating which uses Stannous Chloride and Hydrochloric Acid and
> also had no luck-- it turned the copper I was trying to plate black.
> Perhaps I have Stannic Chloride?  I have no idea how they differ.
>
> Thanks-
> Larry Battraw
>




------------------------------------

Be sure to visit the group home and check for new Links, Files, and Photos:
http://groups.yahoo.com/group/Homebrew_PCBsYahoo! Groups Links

Attachments

Move to quarantaine

This moves the raw source file on disk only. The archive index is not changed automatically, so you still need to run a manual refresh afterward.