On Mon, 12 May 2014 18:25:04 -0400, you wrote: >Any ideas if I am correct of this? Am I merely re-discovering common >knowledge of this list? Are there many people who only use the first >phase due to its insanely fast etch times? > > <snip> This paper is a good place to start: href="http://techref.massmind.org/techref/pcb/etch/CuCl2.htm" Also check old posts in this group; LOTS of discussion of the subject. Keith Bowers WB4LSJ- Thomasville, NC