2016-01-31 by Harvey White

On 31 Jan 2016 05:46:34 -0800, you wrote:

>Probably due to the unmodified laminator I used.  I had to run the board through 5 or 6 times to get good transfer to the board.  Even with rotating the board between passes, I usually had holes on end shifted over about a half pad or more. I also had to run the board through 3 times to preheat before applying the transfer pattern. Total time involved is about the same as when I used the laminator.  Also I had to use a genuine Brother cartridge, could not get good transfer with generic cartridges.  With the cold method I have not had any problems with either type.

Brother has been known to have higher temperature melting point
toners.  This could be a difficulty.  Cold method bypasses that, of
course.  If you go to the hot method, you might experiment with a
transfer from another kind of laser printer.

Harvey


>DuWayne

Attachments

Move to quarantaine

This moves the raw source file on disk only. The archive index is not changed automatically, so you still need to run a manual refresh afterward.