On Thu, 09 Dec 2004 07:35:26 +1100, Adam Seychell <a_seychell@...> wrote: > > The three above mentioned etchants normally have acid and pH will be > very low (< 1). Acrylic (PMMA) is ok for acid. I made a small > electrochemical test cell out of this stuff and have had 20% sulfuric > acid in it for weeks at a time and see zero effect to date. > Nylon is the common plastic you must avoid contact with acid for long > periods, even vinegar. > Of course there is always www.google.com And the links section, where you will find links to chemical compatibility pages. (tank construction folder) ST
Message
Re: [Homebrew_PCBs] Re: Etch safe materials for etch tank
2004-12-08 by Stefan Trethan