Ernst, >> I am down to near the bottom of the quart can of Hydrocote I first >> purchased, and I think I've noticed a viscosity increase. ... >Is there any chance the viscosity increase is actually 'Hydrocote >polymerised' or just solids sinking / solvents evaporating ? One would >expect polymerisation to happen on top of the liquid of course. I think some polymerization is a distinct possibility. I'd be most concerned if it occurred in clumps -- making a smooth application tough. I'm wondering if we ought to stir the mix very well when first purchased and pour it into several smaller bottles. The 4 oz./ 110 ml. ink bottles come to mind as possible candidates. Paul
Message
Re: [Digital BW] Coating (was Faux Meyer Rod - first dMax test results)
2002-12-10 by Paul Roark