Re: [Homebrew_PCBs] Toner Transfer Failures
2012-03-06 by Paul Whatton
+1. I am so glad I don t do toner transfer any more! Paul G4DCV ... [Non-text portions of this message have been removed]
Yahoo Groups archive
Messages
Page 122 of 707 · 35337 messages matched
2012-03-06 by Paul Whatton
+1. I am so glad I don t do toner transfer any more! Paul G4DCV ... [Non-text portions of this message have been removed]
2012-03-06 by chris
... First try: Printed a sample from some packages example, magazine paper, HP P1102W Laser printer. Not too bad, did not fuse well to board though. I started
2012-03-06 by Benjamin Blumer
Another tip: concerning the tedious process of drilling, it won t be as rugged as properly drilling the holes, but you can always try to surface mount your
2012-03-05 by Harvey White
... Either board not clean enough or not enough heat, unless there s a problem with the magazine paper. ... I d have used the scotch brite first (I use
2012-03-05 by Benjamin Blumer
When you say polished it makes me think of a shiny, perfectly smooth surface. I tend to rough my boards up a bit using high grit sandpaper. My logic is
2012-03-05 by michael tenore
Hi! Using a iron to do toner transfer successfully takes some experimentation! You did not indicate the size of the board you are trying to make,But it is
2012-03-05 by tda7000
... The repeated failure to transfer your toner seems rather strange. Certainly it sounds like you have got the board clean enough. I found that for me, making
2012-03-05 by tda7000
... I also use 0.8mm for most things like capacitors, resistors etc. You need 1.0mm for some diodes, TO-220 regulators and such. Some even more. If you re ever
2012-03-05 by Spencer W
I bought this laminator, http://mobile.buy.com/ibuy/Product.aspx?sku=211236158 . $43 for the gbc h212 and get perfect toner transfers. Run it through 6-8 times
2012-03-05 by Leon Heller
On 05/03/2012 20:24, John wrote: Project under planning... The chip fit fine but I ... I use 0.7 mm or 0.8 mm for most parts, including ICs. I often use 0.6 mm
2012-03-05 by John
This has become a humpling experience! You folks have made this sound too easy, or maybe senility has set in on my part. First try: Printed a sample from some
2012-03-05 by Pete
Thanks for the advice folks, a great response to my question and all much appreciated. I ll do some more trials and report back soon. Thanks Pete
2012-03-05 by Leon Heller
... I use Mega Electronics boards, and they seem to go off after about six months or so. Leon -- Leon Heller G1HSM
2012-03-05 by Paul Whatton
Hi Pete Are you are buying your pre-sensitised board from Maplin? Particularly from a store rather than mail-order? The only major problem I have had has been
2012-03-05 by Donald H Locker
Apologies to the O.P. I missed the exposed resist and was thinking toner transfer. Donald. -- *Plain Text* email -- it s an accessibility issue () no
2012-03-05 by Eddie Stassen
I presume this is positive photoresist, in which case it looks like either over exposure or transparencies that are not dense enough. Try adjust you exposure
2012-03-05 by Leon Heller
... Try continuous agitation (I rock the container) in heated etchant. I put the small plastic container I use for etching in an outer container of very hot
2012-03-05 by Malcolm Parker-Lisberg
Pete I would suggest that you are not removing all the resist when you develop your board, they need longer and a good spray rinse. I get similar islands due
2012-03-05 by Terry Jones
Try etching it face up...instead of face down. Etches much cleaner. brush it lightly with a nylon (white brisel ) paint brush after about 15 minutes and you
2012-03-05 by Benjamin Blumer
As mentioned by Donald, heating your etchant helps a lot. I ve lost the link, but there was a white paper published by some company that suggested that heating
2012-03-05 by Andrew Leech
I ve also seen this exact problem from under exposure. If possible agitate / rotate board (or leds) during exposure, to ensure even coverage. You may need to
2012-03-05 by Donald H Locker
I d say a process problem. Agitate more often and more vigourously. The stripes are from the glass beneath the copper - the copper I believe is slightly
2012-03-04 by Pete
Hi, I am trying to etch a small PCB and finding it etches unevenly leaving a small area of copper which is stubborn to remove. Just leaving in the etchant for
2012-03-01 by M A
Hi Could you tell me how to calcuate the ESD in clean room area? Thanks & Regards Mohamed Ali From: blue_eagle To:
2012-03-01 by joe M
Hello Brian, That is some pretty cool stuff you have there. Do you hang around in the #linuxcnc of freenode? Would be cool to get your advice, once I start
2012-02-29 by Brian
Although not exactly what you are asking for, I did build my own CNC system and I do use it successfully for isolation routing of PCBs. True it is not as
2012-02-29 by DJ Delorie
... Nah. I drill two diagonally-opposite pins in both boards, and thread wires through them. They come together pretty accurately that way.
2012-02-28 by ohmware
That link points to a process that s only intended for hole wall activation. You still have to electroplate afterwards to have permanent connections between
2012-02-28 by studleylee
goto http://www.thinktink.com/stack/volumes/volvi/condink.htm
2012-02-28 by Kaelin Colclasure
I have been doing some exploration of this topic on my own, using the Desktop and Buddy ShopBot machines available at the TechShop. Basically my conclusion was
2012-02-28 by joe M
Jay, Get on #linuxcnc or #diycnc of freenode. The folks there are awesome and can get you going. some sample info that I have: ...
2012-02-28 by cary heestand
Have you found the CNCZone.com site? There is an overwhelming amount of information and ideas there. A lot of PCB CNC information too. cary ... From: Jay
2012-02-28 by Harvey White
... PC boards need a high speed spindle for routine and drilling. Low mass, and the tools have a limited life. One estimate is 75 linear feet of machining
2012-02-28 by Robert
you want the pcb-gcode (Eagle) yahoo group for that. This is probably the better place though for all around, drilling could be by cad/cam (Bob-cam or?) but
2012-02-27 by ohmware
I just read something that intrigued me in the book How to Diagnose and Fix Everything Electronic by Michael Jay Geier. He talks about some newer PCBs in
2012-02-27 by Jay
Howdy, homebrew folks. I ve done a bunch of googling, searched the homebrew PCB archives, and the like, and the information I ve been able to find on this
2012-02-26 by Harvey White
... A lot, from what I can see. Minimal: one heater rather than two. Significant: Entire box is made of transparent acrylic. From what I can see, the
2012-02-26 by H. Carl Ott
... I had an older model of the tank. Don t know if there are any design changes on your model. I think I used ammonium persulfate (may have been sodium) in
2012-02-26 by Robert
http://ebookee.org/VHDL-Coding-and-Logic-Synthesis-with-Synopsys_270975.html I was looking for the Synopsis EDA downloads and found this, thought some folks
2012-02-26 by Robert
cool! Robert
2012-02-25 by Terry
A simpler/cheaper alternative to electroless prepping of the holes, that seems to work quite well, is to use graphite laden india ink. Add about 10 grams of
2012-02-25 by Malcolm Parker-Lisberg
Make your own pulsed nitrogen UV laser with tow bits of bent aluminium and fresh air For technical coverage of the UV Nitrogen laser, see:
2012-02-25 by Donald H Locker
Took me a while to find it, so I m posting a link to the directory it s in.
2012-02-25 by Leslie Schwartz
Links some people may feel are worth viewing for ideas or inspiration re: various approaches, I found them interesting, it seems all of the parts to make this
2012-02-25 by Dave M
I recently ran across a booklet that I had bought (online) a number of years ago that describes, in pretty good detail, a process for making PCBs with plated
2012-02-25 by kabowers@NorthState.net
... Another idea from the twilight zone: Could you apply reprap/3-d printer ideas to applying toner? Make an injector with a really fine orifice (ss hypodermic
2012-02-25 by Donald H Locker
costs $60/quart, cures with 385nm UV. Could work. Donald. -- *Plain Text* email -- it s an accessibility issue ()
2012-02-25 by Donald H Locker
Copper is an amazing conductor of heat. Bringing the copper-touching toner to a fusible temperature without the laser-facing top layer vapourising would be
2012-02-25 by boombox666
A optical pickup unit from a blueray player or HD-DVD has a 405nm laser diode with the wavelength optimized optics inside like a collimator, focus actuator and
2012-02-25 by boombox666
Hello Sage, I have done some tryntific tests by exposing a photopositive PCB with the common 405nm laser diodes from HD-DVD and Blueray players. Here are the